Elektroda za zavarivanje čelika tipa 18Cr 12Ni 2.8Mo. Također je pogodna za zavarivanje stabiliziranih nehrđajućih čelika sličnog sastava kada je radna temperatura maksimalno 350 ° C.
Typical Tensile Properties
ISO |
Condition |
Elongation |
Tensile Strength |
Yield Strength |
As Welded |
40 % |
570 MPa |
460 MPa |
AWS |
Condition |
Elongation |
Tensile Strength |
Yield Strength |
As Welded |
- |
- |
- |
Charpy V-Notch Properties
ISO |
Condition |
Impact Value |
Testing Temperature |
As Welded |
60 J |
20 °C |
As Welded |
55 J |
-20 °C |
As Welded |
43 J |
-60 °C |
Weld Metal Analysis
weld metal analysis |
Mn |
Mo |
C |
Si |
Ferrite FN |
Ni |
N |
Cr |
0.6 % |
2.6 % |
0.02 % |
0.8 % |
6 % |
11.0 % |
0.10 % |
18.1 % |
Approvals: |
ABS; E316L-17; BV; 316L; CE; EN 13479; CWB; CSA W48: E316L-17; DB; 30.039.06; DNV-GL; VL 316 L; LR; 316L; NAKS/HAKC; 2.5-4.0 mm; Seproz; UNA 272580; VdTÜV; 00262 |
Classifications: |
EN ISO 3581-A; E 19 12 3 L R 1 2; SFA/AWS A5.4; E316L-17; CSA W48; E316L-17; Werkstoffnummer; 1.4430 |
Approvals are based on factory location. Please contact ESAB for more information.
Alloy Type: |
Austenitic CrNiMo |
Coating Type: |
Acid Rutile |
Ferrite Content: |
FN 3-10 |
Welding Current: |
DC+, AC |