Data sheet

Materijal
Čelik
Proces zavarivanja
REL - elektroda
Prečnik
6,0

Description:

                                                                             Classification:         
                                                                        EN 499:        E 42 4 B 32 H 5
                                                                                                                                DIN 1913:         E 51 55 B 10
                                                                                                                          AWS A-5.1:      E 7018- 1H4R
                                                                                                                                                        EN ISO 2560-A:     E 42 4 B 32 H5
                                                                                                                    EN ISO 2560-B:     E 49 18 A
                  EVB 50
                                
   Description and application:
   Basic, CTOD tested electrode with excellent welding characteristics, recommended for welding structural steels and
   steel castings with tensile strength up to 610 N/mm2 and finegrained steels with increased yield strength.
   Metal recovery is about 118 %. Deposits have very low hydrogen contents (HD < 4 ml/100 g).
   Base materials:
                                  SIST EN    DIN    W.Nr.
   Unalloyed steel    S185 - E335    St 33 - St 60.2    1.0035, 1.0060
   Fine grained steel    S235N - S355N    St E 255 - St E 355    1.0461, 1.0545
                                  P255NH - P355NH    W St E 255 - W St E 355    1.0462, 1.0565
                                   S420ML    TStE 420 TM    1.8836
   Boiler plate    P235GH, P265GH    H I, H II,    1.0345, 1.0425
                                  P295GH, P355GH    17Mn4, 19Mn5    1.0481, 1.0473
   Pipe steel    P235G1TH - P355T2    St 35 - St 52.4    1.0308, 1.0581
                                  L210 - L360GA      St E 210.7     1.0307, 1.0499
                                  L240NB - L415NB      StE290.7 – StE415.7    1.0484, 1.8972
   Shipbulding plate    S235JRS2-S235J4S    GL-A, do GL-E    1.0441, 1.0476
                                  S310G1S – S355G2S    GL-A32 do GL-D36    1.0513, 1.0585
   Cast iron    GE200 – GE260    GS-38 do GS-52    1.0420, 1.0552
   Coating type:        Typical all weld metal properties:
            Basic
                                                        Chemical composition, wt %:
   Welding current:                 
C                                     Si                                    Mn
                                                                 0.07                                 0.60                                1.0
                DC +
                AC (OCV>70 V)
                                                        Mechanical properties:
   Welding positions:                                               As welded                             stress relieved
                     o                                                                                             600 C/ 2h
                                                                                                                                                                       2
                                                        Yield strength    R     / Rp    : > 440 MPa (N/mm )    >440 MPa  
                                                                                                                                                                     2
                                                        Tensile strength Rm:    510 – 610 MPa (N/mm )      510 – 610 MPa
   Redrying temperature:
                                                        Elongation         A5:      > 24%                                  > 24%                        
                400°C / 1 h
                                                        Impact energy   KV :     > 67(typ.100) J (-40°C)        > 67(typ.200) J
        o     /                                                   > 47(typ.100) J (-50 C)
              Hydrogen content: < 4 ml / 100 g weld metal  
                                                    
                                                          Welding and packing data:
                                                             Welding parameters    Packing
                                                               φ      
Length     
Current     
Weight/     
Weight/    Weight/
                                                       mm
                                                       mm           A      Packet      carton    1000 pcs
       Approvals:
                                                                                                         kg          kg          kg   *
        CR:     4YHH    2    300    50 – 70    3.4    17    12.5
        ABS:   4YHH    2.5    300/350    65 – 90    3.4/4    17/20    19.8/23.4
        BV:     4YHH
                                                       3.25    350/450    110 – 140    4/5.4    20/27    36.4/49.5
        GL:     4YH10
                                                         4    450    140 – 180    5.4    27    67
        LR:     3/3YH
                                                         5    450    180 – 230    5.4    27    106
        DNV:   4YH10
                                                         6    450    240 – 290    5.4    27    150
        RS:    3YHH
         SŽ    8    450    350 – 450    5.4    27    275
        TÜV
        DB
        RINA:  4YHH
        PRS:   4YH10